Application de corindon chromé
Chrome corundum has excellent properties and is widely used in high-temperature fields with harsh environments, including non-ferrous metallurgical kilns, glass melting furnaces, carbon black reactors, waste incinerators, etc..
Les matériaux réfractaires contenant du chrome ont de bons effets dans les fours métallurgiques non ferreux en raison de leurs propriétés uniques. Bien que de nombreux chercheurs étudient désormais les matériaux réfractaires sans chrome utilisés dans la métallurgie des non-ferreux, the use of chromium-containing refractory materials as smelting furnace linings in non-ferrous metallurgy is still the mainstream. En outre, chromium-containing refractory materials are also used in zinc volatilization kilns, copper converters, coal gasification furnaces, and carbon black reactors.
Aluminum-chromium refractory materials as lining materials
Aluminum-chromium refractory materials are also commonly used in carbon black reactors, including the combustion section, throat section, reaction section, etc.. Aluminum-chromium refractory materials serve in the ultra-high temperature (19009℃) area of carbon black reactors, chemical erosion areas of reducing gases (C, CO, H2) and ash, and areas with frequent temperature fluctuations.
Donc, the aluminum-chromium refractory materials used in carbon black reactors should have the following characteristics:
- Haut pouvoir réfractaire, température de ramollissement sous charge élevée, and low high-temperature thixotropy rate;
- Stability under a strong reducing atmosphere;
- Strong resistance to molten ash erosion;
- High high temperature strength and anti-scouring performance;
- Bonne résistance aux chocs thermiques
Among the matériaux réfractaires used for the lining of the garbage melting incinerator (ash melting furnace), the refractory materials containing gasified tantalum generally show good corrosion resistance. When the combustion temperature is higher than 1250℃, chrome corundum products are used. The garbage melting incinerator is generally an oxidizing atmosphere, so C-5iC bricks and SiC bricks with poor oxidation resistance cannot be used, and A1203-Cr203 materials and Mg0-Cr203 materials are preferably used. In general, the erosion rate of AI203-Cr203 materials increases with the increase of basicity, so it is mainly used in melting furnaces with relatively low basicity.